Meltings Center
 
  Vacuum Induction Melting Technology
Advanced Technical Scale Production Line
Investment Casting & Supplementary Materials
High Performance Superalloy and Castings
Rare-earth Magnet Alloy Ingot

 
  High Performance Casting Superalloy  
 

...... Casting superalloy is widely used in aviation engine, aerospace engine, gas turbine, ship, metallurgy, petroleum and glass industry for it's super anti-heat, anti-oxidation and anti-corrosion property. BIAM's directionally solidified alloy and single crystal alloy improve the components' operating temperature and thus prolonged the durability and reliability of the components enormously. All kinds of alloy developed by BIAM can match the property of the alloy developed and produced in the advanced countries or even better. So, BIAM's products are widely used in martial industry and civil industry.

 

A comparison of some of the superalloys developed by
BIAM with congeneric products abroad

Types of alloys BIAM's alloys Foreign alloys
Conventional casting superalloys Ni-base alloys K403, K405, K406, K19H C6K, In713C, In100, MM002
Co-base alloys K640, Co-Cr-Mo X40, W152, FSX-44
Cr-base alloys K25 BX-4
DS alloys DZ4, DZ22, DZ125, DZ22B PWA1422, Rene 125DS
SC alloy First generation DD2, DD3, DD4 PWA1480, Rene N4, CMSX-2
Second generation DD6 PWA1484, Rene N5, CMSX-4
Ni3Al intermetallic compound alloys IC6, IC6A, IC10 BKHA-Y

Figure: 140MPa/100h Temperature Capability (13.1Kb)